Gumball
07-20-2013, 11:59 AM
So, as I wrote about on my bodywork thread, I had a few spots where there was gelcoat pockets between layers of fiberglass, causing me to remove a pretty good amount of material in those spots. I'm planning on filling the seams on the body tomorrow (the weather is supposed to be in the low 70s with minimal humidity) and wanted to get some feedback before I start piling on materials.
The largest of the four trouble spots is about 3/4" wide, 2" long, and less than 1/8" deep (actually .101 at the deepest point). Originally, I was thinking that I should fill these with fiberglass (a gooey mixture of chopped mat / flock and resin), then cover with HSRF, then finish off with Rage Gold. After pushing aside bodywork for a day of fun at the racetrack - and plenty of time to think about what I'm about to do, I'm now re-thinking that plan.
Given that these aren't anywhere as bad (meaning deep) as I originally thought, what do you all think about just using HSRF and Rage Gold? I'm concerned that if I also introduce the resin, that's just too many dissimilar materials in a relatively small void - potentially increasing the risk of printing or failure.
Thoughts?
http://i845.photobucket.com/albums/ab15/CCRsAC/Void1_zps3a8aa9ec.jpg (http://s845.photobucket.com/user/CCRsAC/media/Void1_zps3a8aa9ec.jpg.html)
http://i845.photobucket.com/albums/ab15/CCRsAC/Void2_zps5a23539e.jpg (http://s845.photobucket.com/user/CCRsAC/media/Void2_zps5a23539e.jpg.html)
The largest of the four trouble spots is about 3/4" wide, 2" long, and less than 1/8" deep (actually .101 at the deepest point). Originally, I was thinking that I should fill these with fiberglass (a gooey mixture of chopped mat / flock and resin), then cover with HSRF, then finish off with Rage Gold. After pushing aside bodywork for a day of fun at the racetrack - and plenty of time to think about what I'm about to do, I'm now re-thinking that plan.
Given that these aren't anywhere as bad (meaning deep) as I originally thought, what do you all think about just using HSRF and Rage Gold? I'm concerned that if I also introduce the resin, that's just too many dissimilar materials in a relatively small void - potentially increasing the risk of printing or failure.
Thoughts?
http://i845.photobucket.com/albums/ab15/CCRsAC/Void1_zps3a8aa9ec.jpg (http://s845.photobucket.com/user/CCRsAC/media/Void1_zps3a8aa9ec.jpg.html)
http://i845.photobucket.com/albums/ab15/CCRsAC/Void2_zps5a23539e.jpg (http://s845.photobucket.com/user/CCRsAC/media/Void2_zps5a23539e.jpg.html)